Crack filler
副标题
ABUIABACGAAggo2n0gUo3PGWMzDuBTjuBQ

Strong strength Crack Filler material on sales

Material: Polyurethane

Type:Liquid

Color:Light green

Packing:30kg/drum

Brand:GRK

Usage:0.1kg/sqm

Place of origin: Guangdong China


 
Product Information
副标题

concrete crack filler

Decription

It is Single component material. Moisture curing is mainly used in the expansionjoint of cement foundation and the filling or repair of local foundationcracking. In the tensile strength, the product itself has a 10times the stretchand rebound, enough to resist the normal base of the expansion.(Except forfoundation settlement, collapse)

Application

For any concrete base.

Package and Storage

Packing: 30kg /drum

Stored in a cool, ventilated and dry warehouse,keep away from fire and heat sources, and keep waterproof, damp proof and lightproof.

Storage period: six months from the date ofproduction. More than the storage period, the test can continue to use.

Composition

Chemical NameIn % by WeightCAS No.EC No.Molecular Formula
polyurethane resin53%9009-54-5210-898-8C3H8N2O
DOTP13%6422-86-2229-176-9C24H38O4
Calcium carbonate5%471-34-1207-439-9CaCO3
Talc15%14807-96-6238-877-9Mg3[Si4O10](OH)2
iron oxide14%1332-37-2215-570-8-----

Installation

1)   After clean the base, cut the V shape

2)   Apply 1 layers base coat (primer), after dry.

3)   The normal crack ,fill with crack fillermaterial one layer, use trowel to apply one layer by width:500px, thickness1.5mm

4)   Before dry, put the mesh fabric on it.

5)   After dry, polish it.

6)   If the big crack, it suggests to fill ingranule firstly, then pour the crack filler material.